Alan,
How often do you take your reading during a shift??
>>> Alan Kreplick <[log in to unmask]> 03/10/98
09:27am >>>
Wilber,
I use the Wave Solder Optimizer (similar to the Wave Rider). It measures
preheat temperature, and solder pot variables such as temperature,
dwell time,
left-right parallelism & contact time, wave depth.
It has worked out well as a tool to insure the same set-up especially
after
cleaning (removing the solder nozzle during maintenance).
We've set-up control limits on these variables and make corrections as
required
if the readings are out-of-control prior to running production hardware.
Good luck,
Al Kreplick
Teradyne, Inc.
Boston, MA
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|