Michael,

A quick guess is you have smears of solder paste or a paste slump that
leaves a paste web. It might be related to a temp profile that sputters the
paste of drives off the flux before reflow. 

I assume you just started using a new paste from your description, you might
keep searching.

I don't know about the acceptability of small solder balls but they sure
don't look good.

I had an old paper on Solder Beading, see:
www.kondner.com/files/Solder_Beading.pdf  Not exactly what you are seeing,
the beads are typically larger than what paste smears leave. But, it might
help

Bob K.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Forrester, Michael (H
USA)
Sent: Wednesday, November 30, 2011 10:39 PM
To: [log in to unmask]
Subject: [TN] Real World Acceptability of Solder Balls.

I have a PCA 6"X4" with a 144 pin LQFP on it.  The lead spacing is 0.5 mm
which leaves about 0.2 mm space in-between the pins.  The board goes through
SMT reflow and a selective wave.  We are seeing various degrees of solder
balls/spheres.  The balls we see are basically two sizes 40-45um and
70-80um.  The solder paste is a size mesh 3, which would explain the smaller
balls.  At this time I am not sure where the larger ones are coming from?
We see around the LQFP any where from 2-5 balls and literally hundreds of
balls.  The solder paste is a no-clean and then the board is cleaned.  The
reason for using no-clean is because of the process wait time from reflow to
cleaning.  The vendor does not want to leave an aqueous flux on the board
for an extended period of time.
 
My basic question is: Is there an IPC specification(or general rule of
thumb) on the acceptability of solder balls?  I understand that the presence
of solder balls is a process indicator and that IPC-610 states:
 
Solder balls are not entrapped, encapsulated or attached or can become
dislodged in the normal service environment.
 
Does this really mean that if I find a single ball that is not
entrapped/attached, this is a reason for rejection?  Is this practicable or
is there a spec./industry standard that says something like if you have X
balls smaller than X in an area X, this is acceptable?  In the real world,
are companies holding the zero tolerance on solder balls?
Thank you in advance.
 
Best Regards,
 
Michael Forrester
Sr. Product Engineer
CSMTPE
 
Siemens Healthcare Diagnostics
101 Silvermine Rd.
Brookfield, CT  06804
PH: (203) 740-6452
 

----------------------------------------------------------------------------
---
This message and any included attachments are from Siemens Healthcare
Diagnostics and are intended only for the addressee(s). 

The information contained herein may include trade secrets or privileged or
otherwise confidential information. Unauthorized review, forwarding,
printing, copying, distributing, or using such information is strictly
prohibited and may be unlawful. If you received this message in error, or
have reason to believe you are not authorized to receive it, please promptly
delete this message and notify the sender by e-mail with a copy to
[log in to unmask]
----------------------------------------------------------------------------
This message and any included attachments are from Siemens Medical Solutions
and are intended only for the addressee(s). 
The information contained herein may include trade secrets or privileged or
otherwise confidential information. Unauthorized review, forwarding,
printing, copying, distributing, or using such information is strictly
prohibited and may be unlawful. If you received this message in error, or
have reason to believe you are not authorized to receive it, please promptly
delete this message and notify the sender by e-mail with a copy to
[log in to unmask] 

Thank you

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives For additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2