TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 25 Mar 2010 17:07:14 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
From:
Richard Kraszewski <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (293 lines)
If it's a real bad case of co deposition you can tell with a microscope
and solder iron. 

Just touch the tip with a solder iron and watch the melt front as it
progress up the lead. In some instances I have see little volcanoes of
dark material ~exploding to the surface. 

Rich Kraszewski
(920)969-6075

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, March 25, 2010 1:10 PM
To: [log in to unmask]
Subject: Re: [TN] Orange Peel Termination Finish

Hi Joe - is the surface finish bright acid tin? Sometimes the organic 
brighteners in some tin formulations, especially bright acid tin, are 
codeposited and result in weird topography and/or solderability issues 
during solder processing. The "bumpy" connector picture Steve posted 
looked like an example of a codeposited brightener problem.

Dave



"Kane, Joseph E (US SSA)" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
03/25/2010 10:56 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Kane, Joseph E (US SSA)" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Orange Peel Termination Finish






Here's a pretty good scan:

http://ipc-technet.groupsite.com/galleries/photo/117591

-Joe

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US 
SSA)
Sent: Thursday, March 25, 2010 11:34 AM
To: [log in to unmask]
Subject: Re: [TN] Orange Peel Termination Finish

Not blumpy exactly.  I don't have a soft copy of this document, so I'm 
trying to get a good scan.

-Joe 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Thursday, March 25, 2010 11:14 AM
To: [log in to unmask]
Subject: Re: [TN] Orange Peel Termination Finish

Eeeeewwwww... That is ugly!

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, March 25, 2010 10:43 AM
To: [log in to unmask]
Subject: Re: [TN] Orange Peel Termination Finish

Does it look something like this?

http://stevezeva.homestead.com/files/Connector_Blumpies.jpg

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US 
SSA)
Sent: Thursday, March 25, 2010 9:38 AM
To: [log in to unmask]
Subject: [TN] Orange Peel Termination Finish

One of our guys brought over a counterfeit parts manual with a picture
of 
some component leads exhibiting a rough orange-peel texture.  The
picture 
was presented as evidence of re-tinning, which could indicate a 
counterfeit part.

The question is what could cause orange peel finish after hot solder
dip? 
We perform a lot of hot solder dip, both in-house and outside, and
neither 
of us could remember the last time we saw anything like this, though it 
does look kind of familiar.

In the picture, we could see no obvious patches of de-wetting or 
non-wetting, just a uniform pebbly surface.  I don't think this would be

caused by a solderability problem, or rapid cooling, could it be too 
little immersion time in the hot solder?  Could the solder in the pot be

contaminated with something like copper, gold, or iron?

-Joe


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in
the 
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per 
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives 
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in
the 
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: 
send e-mail to [log in to unmask]: SET Technet Digest Search the archives
of 
previous posts at: http://listserv.ipc.org/archives Please visit IPC web

site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815
-----------------------------------------------------


Note: All the information contained in this e-mail and its attachments
is 
proprietary to Kaiser Systems, Inc. and it may not be reproduced without

the prior written permission of sender.  If you have received this email

in error, please immediately return it to sender and delete the copy you

received.



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in
the 
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: 
send e-mail to [log in to unmask]: SET Technet Digest Search the archives
of 
previous posts at: http://listserv.ipc.org/archives Please visit IPC web

site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in
the 
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: 
send e-mail to [log in to unmask]: SET Technet Digest Search the archives
of 
previous posts at: http://listserv.ipc.org/archives Please visit IPC web

site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2