The 50% trace reduction, if that is what you would use also has criteria for
length of trace affected...not sure what the actual area of this particular
defect are but just from the picture, and what I've seen in fabrication in
the past, this is most likely not an isolated defect...I would wager a
closer look at the board will identify other...conditions such as that
shown...
As for vias, or plated through holes as well...current flows through a via
quite different then through a trace...imagine the via squeezed in the
center, sort of like an hourglass...now...pour water through it...thats
about what I believe is happening to current through a trace looking like
that shown...resistance at the point of reduction...of course I could be
wrong...(ducking as the engineers start steaming...)
Franklin
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|