TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Mon, 11 May 2009 07:53:35 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (131 lines)
So are you telling us not to use Al Schneider or no-clean soldering
materials?
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Tellefsen
Sent: Monday, May 11, 2009 6:34 AM
To: [log in to unmask]
Subject: Re: [TN] Parylene Adhesion Tape Test

At Nepcon west 1999, Al Schneider presented some work  I did on Paralene
and no-clean soldering  materials with disappointing results.  If anyone
wants a copy, email me.

Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069



 

             Mary Lou Sachenik

             <[log in to unmask]

             OM>
To 
             Sent by: TechNet          [log in to unmask]

             <[log in to unmask]>
cc 
 

 
Subject 
             05/09/2009 07:59          [TN] Parylene Adhesion Tape Test

             AM

 

 

             Please respond to

              TechNet E-Mail

                   Forum

             <[log in to unmask]>

             ; Please respond

                    to

             Mary Lou Sachenik

             <[log in to unmask]

                    OM>

 

 





We recently had some issues with lack of adhesion of Parylene coating

What types of notes are being used on drawings to define parylene
conformal coating adhesion test on pwa's?
Is the ASTM3359-08 (for assessing the adhesion of coating films to
metallic substrates) the best spec to call out for this testing .
I presently don't have pwb coupons to perform destructive cross hatch
test.

What type of tape is being used testing parylene adhesion on the PWA's?
Some specs call out 3M-250 tape, the ASTM D 3359 calls out the Permacel
99.
Actually I prefer the Wescorp 79210 clear Anti-static Tape, does this
seem
acceptable?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2