TECHNET Archives

February 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ian Hanna <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ian Hanna <[log in to unmask]>
Date:
Mon, 1 Feb 2010 15:19:42 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (136 lines)
But aside from the tin-whiskers mrs lincoln, how did you like the
plating...



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Monday, February 01, 2010 3:08 PM
To: [log in to unmask]
Subject: Re: [TN] [tinwhiskers] Tin Whiskers Threaten US Mint (humor)

LOL that is actually very funny for a very serious subject
 
Copying to technet
 
Technet forum check this out!
 



http://www.youtube.com/watch?v=agSvkoPJHVM

John Burke

(408) 515 4992

 

 

  _____  

From: [log in to unmask]
[mailto:[log in to unmask]] On Behalf Of Brusse, Jay A.
(GSFC-560.0)[QSS GROUP INC]
Sent: Monday, February 01, 2010 8:02 AM
To: [log in to unmask]
Cc: [log in to unmask]; Leidecker, Henning W. (GSFC-5600)
Subject: [tinwhiskers] Tin Whiskers Threaten US Mint (humor)



http://www.youtube.com/watch?v=agSvkoPJHVM

Turn UP the volume!

 

Dear Whisker Fanatics,

 

And now for a moment of levity.

 

I am the proud owner of the US penny shown in the above video.  The
video is
my creation while the penny is the creation of Lyudmyla Panashchenko who
received her master's degree in Dec. 2009 from the University of
Maryland
where she carried out research on tin whiskers.  To create this whisker
treasure Lyudmyla used plater's tape to mask off all but Lincoln's beard
on
the penny.  She then proceeded to electroplate the beard in her lab
using a
pure tin plating bath from which she had previous success growing
whiskers
in support of her research.   As you can see from the video Abe really
needs
a new razor & those who might unwittingly handle such a coin might be in
need of a tetanus shot ;)

 

On a bit more serious note, some additional "whisker-related" videos can
be
found here:

http://www.youtube.com/results?search_query=jaybrusse
<http://www.youtube.com/results?search_query=jaybrusse&search_type=&aq=f
>
&search_type=&aq=f

http://nepp.nasa.gov/whisker/video/

 

Regards,

 

Jay Brusse

Sr. Components Engineer

Dell Perot Systems

NASA Goddard Space Flight Center

 

Phone:  301-286-2019

Fax: 301-286-9778

[log in to unmask]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2