TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jack Olson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Mon, 31 Oct 2011 09:12:16 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (34 lines)
hmmm... 
that response implies that I should probably quit worrying about it, 
since there's not much I can do about that. 
(except maybe conformal coating)

"what, me worry?"
alfred e. newman


.
On Sat, 29 Oct 2011 10:10:08 -0400, Terry Munson <[log in to unmask]> wrote:

>We have found whiskers from the sac 405 and 305 solders. And Celestica published a paper on there experiments last year showing whiskers on solder joints as well. 
>
>Terry Munson 
>Foresite 
>765-457-8095
>
>
>On Oct 28, 2011, at 4:52 PM, Joyce Koo <[log in to unmask]> wrote:
>
>> It depends.... 
>> http://www.atotech.com/data/publications/pcb/Immersion_Tin-Kinetics_of_Whisker_growth.pdf

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2