Friends:

I have a 6 layer board that warps.  The R&D group tells me its a
Manufacturing problem. I'm not so sure.

Details:
.062" Thick NEMA FR4
Stack: (Trace/Gnd/Trace/Trace/Power/Trace) w/1/2 oz copper clad.
R&D group tells me the layers are balanced from the center of the stack
out.

What should Manufacturing be doing to prevent these boards from
warping?  Or is the only solution a higher temperature
FR4 material that adds cost to the board.  Could it be a problem with
the board house. Please advise.

Regards, Chris

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2