TECHNET Archives

September 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Grunde Gjertsen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Grunde Gjertsen <[log in to unmask]>
Date:
Thu, 18 Sep 2014 07:39:35 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (47 lines)
The Immersion gold is not only very thin but it's also very pure hence soft, insertion is one thing but what about fretting over time?
Personally I'd stay away or at least be very careful about testing, depending on the environment reliability will suffer and it's a far cry from the PCI spec.


Grunde Gjertsen | Project Manager
Kitron AS, P O Box 799, NO-4809 Arendal, Norway
Phone: +47 92405898
Fax: n/a
[log in to unmask] | http://www.kitron.com
________________________________________



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Carl VanWormer
Sent: 18. september 2014 00:14
To: [log in to unmask]
Subject: [TN] can ENIG be used for PCB card edge fingers?

We have a PCI Express card edge connector that accepts a PCB with Gold plated fingers.  The hard Gold plating costs extra money.  Since the board will only be plugged into the connector a few times, it was suggested that we just use an ENIG plated PCB.  The ENIG is a much thinner plating, compared to the hard Gold plating usually used for PCB edge connectors.  I've been unable to locate information on this choice.  Have any TechNetters tried this cheap approach?  I'm looking for success or failure stories to add to our discussions.

Thanks,
Carl



Carl B. Van Wormer, P.E., AE7GD
Senior Hardware Engineer
Cipher Engineering LLC
    21195 NW Evergreen Pkwy Ste 209
    Hillsboro, OR  97124-7167
    503-617-7447x303
    [log in to unmask]<mailto:[log in to unmask]>     http://cipherengineering.com<http://cipherengineering.com/>

This message may contain confidential and/or proprietary information, and is intended for the person/entity to whom it was originally addressed. Any use by others is strictly prohibited.  If I sent this to you by mistake, please be nice and delete it, and then tell me of my mistake so I can send it to the right person.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2