Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vI6ct-0000QzC; Mon, 28 Oct 96 23:22 CST |
Old-Return-Path: |
|
Date: |
Mon, 28 Oct 96 10:15:59 PST |
Precedence: |
list |
Resent-From: |
|
From [log in to unmask] Thu Oct 31 16: |
32:52 1996 |
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"Zk8jN.0.pT6.2IPTo"@ipc> |
Subject: |
|
From: |
|
Cc: |
|
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Do you refer to "permanent" solder mask (ie. applied by PWB vendor) or
temporary solder masks (that you apply and either "wash off" or
manually remove)?
I can go into our experiences if you want to call or email me
directly.
Jim Maguire
Senior Principal Engineer
Boeing Defense & Space Group
PO Box 3999 M/S 3W-97
Seattle, WA 98124-2499
Phone 206-657-9063
FAX 206-657-8903
Email: [log in to unmask]
______________________________ Reply Separator
_________________________________
Subject: Alternative Solder Masks
Author: [log in to unmask] at esdigate
Date: 10/25/96 7:59 AM
I need some information on alternative solder masks to be
used with no-clean flux. Protecting tooling holes as the
CCAs are processed across the wave solder machine is the
concern. We are considering Kester 973 VOC flux and Kester
951 no-clean flux. We solder in panels, half panels, and
single boards. I am expecting the machine to automatically
control wave height to prevent flooding, etc. Could I
please get some feedback on the mask issue since I will be
doing some tests on some machines in the immediate future.
Thanks in advance!!!
My address is [log in to unmask] if you want to contact me
direct.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|