TECHNET Archives

April 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 2 Apr 2004 13:17:56 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Steve Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (50 lines)
Hi David!

Not sure quite you mean when you say; "Pre-formed tab to add extra volume to
the spheres." Can you elaborate further?

You also say that you want to avoid adding solder paste, can I ask why? If
the ball-pitch, ball count, and ball pattern is pretty standard, you can buy 10
Flextac stencils from Circuit Technonolgy Center for around $50. They work
wonderfully too! Go to:

http://www.circuittechctr.com/products/201-3120.shtml

and check them out. I've got pictures up on my page of me using one to solder
a Power PC BGA to a SMT-to-PTH adapter, which I'm sure if there wasn't
something like Flextac stencils around, would have been a real bear to do.

Give us a few more details...

-Steve Gregory-


> Hello Technetters,
>
> I have some BGA sockets which I am trying to solder to PCBs.
>
> The sockets have stand-offs which prevent the solder spheres from collapsing
> and making a good mechanical/electrical connection.
>
> Ideally what I am looking for is a pre-formed tab to add extra volume to the
> spheres.  I do not have an in-house machine shop to make a stencil to apply
> paste and quite frankly I would like to avoid that course if possible.
>
> Thank you in advance for your help,
>
> David Tremmel
> Technical Manager
> Belmont Component Services
>


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2