Here are the ASTM specs for determining porosity:
Standard Test Method for Porosity in Gold Coatings on Metal Substrates
by Nitric Acid Vapor, B735-89.
Standard Test Methods for Porosity in Gold Coatings on Metal
Substrates by Paper Electrography, B741-90.
Standard Test Method for Porosity in Metallic Coatings by Humid Sulfur
Vapor ("Flowers-of-Sulfur"), B809-90.
Standard Guide for Selection of Porosity Tests for Electrodeposits and
Related Metallic Coatings, B765-86.
Editorial comments - These are all subjective tests designed to "decorate"
pores in noble platings for determining the degree of porosity. They do
not have acceleration factors such as x hours in the nitric acid
environment = x hours in the field. You have to look to MFG testing for
that. Enjoy!
Rod Martens
Hewlett-Packard.
______________________________ Reply Separator
_________________________________
Subject: Re: [TN] Contact resistance
Author: Non-HP-ddhillma ([log in to unmask]) at
HP-ColSprings,mimegw4
Date: 3/12/98 6:47 AM
Hi Gaby - you could use SERA to determine the extend of the gold plating
porosity but it won't tell you anything direct about contamination. Give
Mike Pavlov or Peter Bratin an email at [log in to unmask] for more help. I
have had some success and some failures using the SERA tester for noble
metal porosity. You could also use the fuming nitric acid test to determine
your level of plating porosity (hey TechNet - anyone know the ASTM method
number for the test?) but the test is somewhat subjective. You might also
conduct a Scanning Electron microscopy analysis to see what the level of
porosity is plus grab some compositional info - you might be able to find
some contamination this way. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
[log in to unmask] on 03/11/98 05:06:37 PM
Please respond to [log in to unmask]; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject: [TN] Contact resistance
Dear Technetters!
We experience high contact resistance on keyboards.
The plating is 0.15u Au on 6u Ni.
1.Could I use SERA in order to see if there is a contamination on the
keypads
in comparison to the bare boards?
2.If YES, HOW?
3.How could I compare the porosity of the gold plating of two different
batches ?
Thank you in advance
Gaby
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional inform
ation.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-97
00 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|