Hi Ed,
I believe the phenomenon you have is called "creep" or relaxation.
Good luck,
Gerry
> Date: Wed, 15 May 2013 15:57:28 +0000
> From: [log in to unmask]
> Subject: [TN] Elastic/plastic deformation of thermoplastic transistor housing
> To: [log in to unmask]
>
> I have run across an interesting phenomenon and was hoping someone has done exhaustive research on it in Technet-ville.
>
> I have a TO-3PF style package (plastic power transistor with plastic tab) that has a specific torque requirement and thread-locker material (microsphere type). When the subassembly is first assembled in a fixture to align the transistors to the heatsink and hold the nut in rotational place then torqued, they are verifiably tightened correctly. Once they sit for a day or so, they are no longer tight and the screw/nut spins in situ together. To my amateur eye, it seems the thermoplastic is exhibiting elastic deformation at this point. If re-torqued again, it stays put, which seems to possibly have crossed the threshold from elastic deformation ("bending" the atomic structure) to plastic deformation ("shearing" the atomic structure).
>
> Is there any insight I can harvest before my 1:00 meeting today?
>
> Ed Popielarski
> Engineering Manager
>
> [Description: FullLogo]
> 970 NE 21st Ct.
> Oak Harbor, Wa. 98277
>
> Ph: 360-675-1322
> Fx: 206-624-0965
> Cl: 949-581-6601
>
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|