Tom,
You might give a call to Ed Small of Multicore (609-488-7191). Ed deals alot
with their MUST-II solderability tester (a wetting balance) and may know of a
source for the coupons you describe. Kester, who also manufacturers a
wetting balance, may have a source.
Doug Pauls