Tom, You might give a call to Ed Small of Multicore (609-488-7191). Ed deals alot with their MUST-II solderability tester (a wetting balance) and may know of a source for the coupons you describe. Kester, who also manufacturers a wetting balance, may have a source. Doug Pauls CSL