TECHNET Archives

September 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Date:
Thu, 30 Sep 2010 09:22:01 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (102 lines)
 Hi Victor,
Here is Tom's e-mail address: [log in to unmask]

 


 Werner

 

-----Original Message-----
From: Victor Hernandez <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, Sep 30, 2010 8:48 am
Subject: [TN] Where about of  "Tom Clifford"


   I did not receive a response to my original inquiry, so I post it again.   
Perhaps someone out there has the article I am searching for  written by Tom in 
the June issue of 2004 of Printed Circuits Board..

Round the clock: a coupon's actual mis-registration is always worse than can be 
seen in any single mount's cross-section


Victor,

_____________________________________________
From: Hernandez, Victor G
Sent: Wednesday, September 29, 2010 12:30 PM
To: TechNet E-Mail Forum
Cc: Hernandez, Victor G
Subject: FW: Round the clock: a coupon's actual mis-registration is always worse 
than can be seen in any single mount's cross-section.
Importance: High


Fellow TechNetters:

   Searching for the where about of Tom Clifford or viewable, with 
images/Figures, link to his above stated article from Printed Circuit Boards.

Victor,

_____________________________________________
From: Hernandez, Victor G
Sent: Wednesday, September 29, 2010 12:24 PM
To: [log in to unmask]
Cc: Hernandez, Victor G
Subject: Round the clock: a coupon's actual mis-registration is always worse 
than can be seen in any single mount's cross-section.
Importance: High


Tom,

        Ref:    Tuesday June 01. 2004

   Can you share the above stated article you wrote back on 2004.   I am most 
interested in the cross section images/photos.   Very interesting article!

   I advance I thank you for your timely response in this matter.

Victor,


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2