TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Thu, 16 Jan 1997 21:01:25 +0800
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9292
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"a5xDH1.0.xTE.khYto"@ipc>
Subject:
From:
Poh Kong Hui <[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vkrjL-0000SHC; Thu, 16 Jan 97 07:19 CST
From [log in to unmask] Thu Jan 16 10:
54:04 1997
X-Mailer:
Windows Eudora Pro Version 3.0 (16)
Message-Id:
Parts/Attachments:
text/plain (26 lines)
Hi Technetters,

I am wandering anyone could suggest ways to get rid of solder skips.

We have a lot of solder skip on the Tant capacitor, case size type A 
and B, but don't have any problem with the rest of the chip components 
and SOICs. The pad size for the Tant Cap id pretty small, only allow 
very little for space for the chip wave to be able to solder to the
terminations.

Any ideas how to fix it..We are running no-clean using a full-blow  nitrogen
tunnel wave-solder machine.


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2