TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Alain Savard <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 19 Dec 2000 12:37:26 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
Hi all,

I haven't looked at plugging on one side for OSP before, but it doesn't
sound like a good idea. Plugged vias have a tendency to entrap chemicals
(from ANY of the subsequent process).  These chemicals can thereafter go
right through the OSP (which typically does not provide very good long term
corrosion protection at any rate) and corrode the material of the vias. For
OSP, I would definitely suggest plugging on both sides or not at all.

Just my 2 cents (that's 3 cents in Canadian money)!

Happy holidays,

Alain Savard, B.Sc.
Chemical Process Analyst
CAE Electronics Ltd.
e-mail: [log in to unmask]


-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: December 19, 2000 10:53 AM
To: [log in to unmask]
Subject: [TN] OSP PROCESS


 Season's Greetings to All
On boards with plugged vias (one side only) that have an OSP coating, does
the
OSP coating go on Before or After the solder mask plugging?

We have boards with corroded holes that I am told have the vias plugged,
then
the board goes through a dilute sulphuric acid microetch, followed by OSP.

Doesn't seem a like a real good idea to me!!

Susan Mansilla
Robisan Lab

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2