TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 10 Oct 2007 16:44:16 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (27 lines)
Hi Phil,
You did not say how thick your PWBs are, but I surmise they are thick.
Removing the thermal reliefs is likely to cause you soldering problems—they 
are there for a reason. 
For SAC soldering, you need more Cu for the via barrel walls because of the 
higher Cu dissolution rate of Cu in SAC. "100% barrel fill is desired with a 
good fillet top and bottom" implies filling with solder; besides poorer wetting, 
you really need to have the T's high enough—that is likely to cause some 
problems with your PWB resin system.

Werner



**************************************
 See what's new at http://www.aol.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2