Thanks Rueven!
I was not even considering the size of BGA balls or package. It is good to know this can be a factor.
Best regards,
Raye Rivera
QA Manager * Canoga Perkins * 818-678-3872 * [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Reuven Rokah
Sent: Thursday, March 01, 2012 1:16 PM
To: [log in to unmask]
Subject: Re: [TN] BGA Reverse Backwards Compatibility
The size of the BGA balls is a factor on the decision for yes/no using mix
process.
Small balls and small thermal body mass of SAC BGAs, can be used in mix
process / mix profile.
I have years of experience without failure report from field but still it
is recommended to SAC process for SAC BGAs and Sn/Pb process for Sn/Pb BGAs.
Reuven
On Thu, Mar 1, 2012 at 10:22 PM, Harp, Ken <[log in to unmask]> wrote:
> Is this for a Hi-Rel application? If so, first recommendation would be to
> go for SnPb paste and profile for an SnPb BGA, and beg for a RoHS
> exemption. If you must go SAC, I'd recommend having the BGA balled SAC
> from the factory and make sure they are kept dry throughout the
> manufacturing process.
>
> With respect to the mixed method, I would side with your engineers.
>
> I'm sure opinions will vary...take this with a grain of salt!
>
> Ken Harp
> Principal Mechanical Engineer
> Astronics Advanced Electronic Systems
> 9845 Willows Road NE, Redmond, WA 98052-2540
> Office: 425.376.4423
> [log in to unmask]
>
>
>
> -----Original Message-----
> From: Rivera, Raye [mailto:[log in to unmask]]
> Sent: Thursday, March 01, 2012 12:11 PM
> To: [log in to unmask]
> Subject: [TN] BGA Reverse Backwards Compatibility
>
> Hello TechNet Gurus.
>
> I have seen lots of discussion and studies on the reliability of using
> BGAs with SAC solder balls on an assembly with SnPb paste. Many people are
> interested in this topic because of backwards compatibility issues when
> SnPb BGAs aren't available. At the risk of oversimplifying a complex topic,
> I understand this can be successful using a backward compatibility thermal
> profile such as the one shown on Figure 8-20 of IPC-7095B to ensure
> complete melting of both types of solder. Of course we must take care that
> the profile does not exceed the temperature limitations of the SnPb paste.
>
> Is anyone aware of any study done on the reverse situation? That is, SnPb
> BGAs used with SAC solder paste and a SAC thermal profile? I would think it
> would be at least as reliable as the above situation. We definitely get
> complete melting and the temperature profile is correct for the SAC solder
> paste chemistry so we are not as concerned about holding a narrow process
> window.
>
> This is not just academic curiosity on my part. We have some prototype
> boards built with SnPb BGAs SAC paste, and SAC profile. They are not for
> sale to customers, but some of our engineers are of the opinion that any
> mixed process joint is suspect. I'd like to find some data on the topic.
>
> I hope everyone is enjoying Apex.
>
> Best regards,
> Raye Rivera
>
> QA Manager * Canoga Perkins
> 20600 Prairie Street * Chatsworth * CA 91311-6008
> 818-678-3872 * [log in to unmask]
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
--
Best Regards,
*Reuven Rokah*
Mobile: 972-52-60-120-18
Tele-fax: 97239360688
<http://www.rokah-technologies.com/>[log in to unmask]
[log in to unmask]
www.rokah-technologies.com
**
This e-mail message is intended for the recipient only and contains
information which is CONFIDENTIAL and which may be proprietary of Rokah
Technologies. If you have received this transmission in error, please
inform me by e-mail, phone or fax, and then please delete all of the
original files and all other copies exist.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|