TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Thu, 15 Mar 2007 18:23:07 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (80 lines)
Agree with Trikeman, the semi process is a epitaxial process using 
"refractory" metal, and the asperity is not measureable on normal 
tallysurfers, i.e. <0.1 um.  Only situation may be with semi chips with 
plated bond pads, but then we talk gold. And these have never caused us any 
problems either. You needn't bother. /Inge

----- Original Message ----- 
From: "Creswick, Steven" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 15, 2007 1:36 PM
Subject: Re: [TN] Gold Ball Bond attaching surface roughness


Victor,

Sorry, don't have a number to give you.  We do it all day long ... and
the IC mfr's know how to make the bond pads....

Typically smoother is better, but if one were to look at the plating on
a lead frame at high enough magnification, it is certainly not smooth
either.

Possibly someone has some form of spec on the surface finish of a bond
pad.  All that I am aware of is pad thickness.

If no one has a surface finish number, I might be able to run some next
week.

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Thursday, March 15, 2007 8:25 AM
To: [log in to unmask]
Subject: [TN] Gold Ball Bond attaching surface roughness

Fellow TechNetters:

Typically I have observed ball bond attached the alunium window of a
chip, and copper lead frame.   Are there any criteria for the roughness
of this surface for establishing a good intermetallic formation?

Victor,

-----------------------------------------------------

THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT 
FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR 
THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the 
intended recipient, you are hereby notified that any review, distribution, 
or copying of this communication is strictly prohibited.  If you have 
received this communication in error, please immediately notify the sender 
by return e-mail, and delete this e-mail message and any attachments from 
your computer.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2