TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Wed, 6 Dec 2006 17:27:01 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
R&D Assembly
MIME-Version:
1.0
Parts/Attachments:
text/plain (108 lines)
From the Deming Dimension:

Point 4. End the practice of awarding business solely on the basis of price
tag. Instead, require meaningful measures of quality along with Price. Aim
to minimize total cost, not merely initial cost.

Point 11. Eliminate work standards that prescribe quotas for the workforce
and numerical goals for people in management. Substitute aid and helpful
leadership on order to achieve continual improvement of quality and
productivity.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, December 06, 2006 4:43 PM
To: [log in to unmask]
Subject: Re: [TN] Counterfeit Part Alert!

However, nothing in the company Christmas stocking for you, Steve, because
you failed to meet your rework reduction goals.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Maxwell
Sent: Wednesday, December 06, 2006 3:41 PM
To: [log in to unmask]
Subject: Re: [TN] Counterfeit Part Alert!

Steve,
And the purchasing people will still get their cost savings bonus this year.

John Maxwell


>Hello All!
>
>Today is my first day back at work after a two-week vacation at home in

>North Carolina, and I had this hit me in the face this morning:
>
>http://stevezeva.homestead.com/files/Allegro_Marking.jpg
>
>We build an assembly that uses an Allegro UCN5801A (0.5 A LATCH BASED
>PRPHL DRVR, PDIP22), and as you see the marking on the part has started

>peeling off. This was after one aqueous wash.
>
>I called Allegro and spoke to an engineer there, and their parts are
>normally laser marked...so they've either been counterfeited, or been
>badly remarked for some odd reason.
>
>So now at seven per assembly, we have a bunch of rework to do...(I
>shoulda stayed home).
>
>-Steve Gregory-
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

>additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2