Sounds like you are using the wrong catalyst. Too short of a pot life or
working life, causing it to set up in the screen.
Hysol makes a two component screenable epoxy marking ink. Their Cat-L-Ink
50-000 series. It is available with a variety of catalysts to control how
fast and at what temperature it cures. It is available in a many colors
including red.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, October 25, 2002 12:36 PM
To: [log in to unmask]
Subject: [TN] Red Ink
Folks, can anyone direct me toward a supplier of red ink suitable for
screening legends onto bare boards? I''m reaching wits end on the 2 part I'm
using....after ½ hour of a run it becomes necessary to wipe the screen out
with solvent which leads to even more issues. Any help appreciated. Peaceful
weekend to you all. ---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or
contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|