TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Crowhurst, Dave" <[log in to unmask]>
Date:
Thu, 18 Sep 1997 09:49:25 -0600
Content-Type:
multipart/mixed; boundary="---- =_NextPart_000_01BCC418.26E6CB50"
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, "Crowhurst, Dave" <[log in to unmask]>
Parts/Attachments:
text/plain (641 bytes) , application/ms-tnef (9 kB)
We are using Kester R 244 62 36 2 solder paste in a double sided
process. Reflow is with forced air and IR in pre heat 1 and the REFLOW
zone, bottom side only (ETC 4 zone oven). The PCB's are manufactured
with the immersion gold process. I am experiencing frosty looking
solder joints. We have attributed this to the gold and silver
contaminants in the solder fillet. This has not effected the
performance of the PCB. Any suggestions or comments.
Thank You

Regards,
[[ MAPI 1.0 storage : 3868 in WINMAIL.DAT ]]

Dave Crowhurst
S.M.T. Process Support
Manufacturing Engineering
Harris Canada Inc.
Wireless Access Div.
Phone (403) 295-5026
Fax      (403) 295-8862



ATOM RSS1 RSS2