TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Terrym <[log in to unmask]>
Date:
Sat, 2 Mar 2013 22:39:23 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (25 lines)
We have seen this when the rinses prior to soldermask were only turned on one side. Or plugged nozzles or even to fast of belt speed.  Contact me off line if you want a copy of a paper I wrote on this issue. The residue causing the blisters typically are sulfate residues.


Terry Munson's iPhone 
Foresite Inc 
765-457-8095. 


On Mar 2, 2013, at 6:13 PM, Ramakrishnan Saravanan <[log in to unmask]> wrote:

> Dear all,
> 
> We have received few MLBs from a contract supplier. The board was inspected and accepted for wiring. The assembly is for high reliability applications. We conformal coated, tested,thermal cycled and closed the package. We opened the package for some rework, we found corrosion under solder mask on some tracks. 
> 
> The corrosion is in the form of  blisters and localized. Center of the tracks or edge or localized and not covering the entire width of the tracks. 
> 
> What could be the reason for corrosion under solder mask ?. How to diagnosed for root cause analysis ? regards,
> 
> R.Saravanan

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2