Dear TechNetters,
We were observing some solderability issues in laminate based QFNs. The solderable terminations were plated with ENIG( Electroless Nickel, Immersion Gold). SEM/EDX analysis showed Nickel plating cracks on the terminations. I have requested Steve Gregory to post the image on his website. If the experts can shed some light on the failure mechanism, I will appreciate it.
Thank-you,
Mumtaz
858-795-0112
CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|