Steve: No, it will decompose at those times and temperatures. Can you use a
lower temp bonding agent? You might be able to get away with 200 F for 30
minutes depending on what flavor ENTEK you're using.
Of course a lot depends on what type of flux, duration and the number of
thermal exposures it will see in assembly.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Steve Kelly [mailto:[log in to unmask]]
Sent: Friday, June 25, 2004 12:13 PM
To: [log in to unmask]
Subject: [TN] OSP Question
Good afternoon,
I have a question on the thermal characteristics of Entek OSP. We have a
flex circuit which requires OSP as the finish. We intend to do the OSP
operation but then we have to thermally bond a rigid stiffener on the flex.
OSP will see pressure and a temperature of approx. 350 F for 1 hour. Will
the OSP handle this. Thanks for your help. Regards Steve Kelly
PFC Flexible Circuits Limited
Ph: (416) 750-8433
Fax: (416) 750-0016
Cell: (416) 577-8433
E-Mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|