Hi Franklin,
Ionic contamination has nothing with type of oxide preparation, only with
the quality of rinses.
From my own experience , we had in the past two  types of oxides ( brown and
reduced black) and now we are running one of replacements - all types of
oxides passed ionic contamition tests nicely.
Edward

Edward Szpruch
Eltek Ltd
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel  ++972 3 9395050 , Fax  ++972 3 9309581
e-mail   [log in to unmask]

> -----Original Message-----
> From: Franklin D Asbell [SMTP:[log in to unmask]]
> Sent: ה דצמבר 05 2002 0:18
> To:   [log in to unmask]
> Subject:      Re: [TN] ionic contamination
> 
> With that black oxide I don't see how they would pass ionic contamination.
> We use an oxide alternative (the exact chemistry I don't know the name of,
> the lab guys do...) and since we made that switch we've never had a layer
> even register on the contaminate scale.
>  
>  
> 
>       ----- Original Message ----- 
>       From: Fineline Circuits, Inc. <mailto:[log in to unmask]> 
>       To: [log in to unmask] <mailto:[log in to unmask]> 
>       Sent: Wednesday, December 04, 2002 7:06 PM
>       Subject: [TN] ionic contamination
> 
>       Hi Fellow Technetters:
>       I would like to know if  there is a process to clean inner layers
> for ionic contamination. Generally we drill, laminate, expose,develop,
> inspect, etch, blackoxide, bake and press inner layers. Its a multilayer
> board we are building for military and requires no ionic contamination
> between layers. (inner or outer).
>       Regards
>        
>       Sona
>        
>        
>        
>       --------------------------------------------------- Technet Mail
> List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe,
> send a message to [log in to unmask] with following text in the BODY (NOT
> the subject field): SIGNOFF Technet To temporarily halt or (re-start)
> delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or
> (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of previous posts
> at: http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/html/forum.htm for additional information, or contact
> Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ----------------------------------------------------- 
> 
> --------------------------------------------------- Technet Mail List
> provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send
> a message to [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery
> of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of previous posts
> at: http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/html/forum.htm for additional information, or contact
> Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2