TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Brian Ellis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Mon, 15 Jul 2013 16:35:27 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
In order, the most probable first:
- the underlying copper has not been correctly cleaned before applying 
the OSP
- the underlying copper has been brushed, pumiced or otherwise treated 
with an abrasive
- the underlying copper, if electrolytic, has been deposited from a 
badly controlled/filtered solution, causing co-deposits of organic 
additives or simply particulate contamination
- your OSP has passed its sell-by date

Brian

On 15.07.2013 14:19, Lyon Yuan wrote:
> Hi All,
>
>
>
>
>
> What are all the probable causes of non-wetting for OSP board test pads when
> the circuit boards are run through reflow?
>
>
>
>
>
>
>
> Lyon Yuan
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2