Larry,
This formula was suggested to me recently for soldering an ENIG board, but
in the end 63/37 was found to be suitable. I was told that the silver
content improves the chances of good wetting on Nickel.
Pete Duncan
Larry Koens
<lwkoens@EIMI To: [log in to unmask]
CRO.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Sent by: Subject: [TN] solder paste with 2% silver
TechNet
<[log in to unmask]
ORG>
07/26/01
04:10 AM
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
Larry Koens
Got a question for everyone,
I just switched companies and the new company that I'm with now uses a
62/36/2 solder paste. I've always used the 63/37 formula. The guys who
decided to use the 2% silver are no longer with the company. My question
to you is, why would they want the 2% silver in the paste? They know
something I don't?!
Thanks,
Larry
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|