TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Campbell, William (wcampbel)" <[log in to unmask]>
Date:
Mon, 11 Dec 2000 09:29:04 -0500
MIME-Version:
1.0
X-To:
"Horaud, Walter" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Campbell, William (wcampbel)" <[log in to unmask]>
Parts/Attachments:
text/plain (39 lines)
Hi Walter-

I got one kind response from someone who has seen a demo and will be getting
a new machine in Feb.  So far they like it, but don't have it yet.

Could you explain which setting can give you trouble? (height, sensitivity?,
etc) ie what does that setting control?

Also wondering, how do you store your squeeggee assemblies?

Thank you (both) for writing!  I was wondering if it was my breath or
something...  ;-)

Bill C.


-----Original Message-----
From: Horaud, Walter [mailto:[log in to unmask]]
Sent: Monday, December 11, 2000 4:09 AM
To: [log in to unmask]
Subject: Re: [TN] formflex tooling


Does anybody give you an answer about formlex tooling ?
We have a formflex tooling on one of our infinity DEK.
We have already done some trials. Inconclusive.
Most problem are due to the setting.

Walter.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2