On cross-sectioning a PWB, I'm finding voids between the metal of the SMT
pad and the main body of the epoxy filled via.
Its a typical resin filled via on a multilayer board.
Where or what are the specs for the voiding in the resin interms of size
etc. and the consequences of these voids?
Thanks in advance
Moss
##############################################################