Jin-Ho -

    I would recommend looking at a different PCB supplier because when we looked at immersion gold, our PCB
fab house told us there was no price difference.  Check it out.

Ryan Jennens
Phoenix Engineering Design

Jin-ho Lee wrote:

> Could you share test data regarding solderability on each
> condition with me. From our beaker test Omikron White Tin
> showed better result than Dexter's. And what about cost
> factor ? As far as I know, if HASL has 1X,  0.6 X for OSP,
> 1.4 X for Tin and 4.0 X for Immersion Gold.
> There is a tendency towarding Immersion Gold, but in the
> standpoint of PCB shop too much burden because most
> our customer want us kept same price as HASL's. In that
> case we have to loose our profit at least $1.0/board ( $
> 10/ sq. meter).So White Tin seems to me very attractive.
> I
>
> J.H.Lee
> R & D Director
> Daeduck ELectronics Co
> [log in to unmask]
> fax: + 82-345-81-8246
> tel : + 82-345-81-8191
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2