I have seen this in the past and you must be very careful during
de-panellising PCBs as well.
We banned 'v' scoring of FR4 surface mount PCBs because of the risk of
cracking surface mount capacitors. The time to failure can be anything from
hours to months depending on environment - temperature, moisture etc.
I have another question - has anybody out there seen chip capacitors fail
open circuit when operated in a circuit which runs quite hot?
Can the end caps become loose through temperature cycling causing the
capacitors to go open circuit at elevated temperatures?
Neil
-----Original Message-----
From: KK Chin [mailto:[log in to unmask]]
Sent: 05 October 2001 17:15
Subject: Re: Leaky Capacitors
We has banned manual soldering for leadless chip capacitors. Years ago we
experienced exactly the same problem. Microsectioning revealed that cracks
are
formed across several layers of the interleaved electrodes. Even bigger
problem
was that the cracked capacitor would not be detected in the initial test.
After
operating for a while, metal migrated across the crack and shorted the
layers.
We glad the problem was caught in burn-in rather than in the field. The
shorted
capacitor burnt some of our assemblies badly.
Manual soldering was not the only cause of capacitor cracking. AVX and Kemet
published some articles about precautions in design and assembly processes.
K.K. Chin
Artesyn Technologies,
Fremont, CA
#####################################################################################
Attention:
This message is for the named person's use only. It may contain confidential,
proprietary or legally privileged information. No confidentiality or privilege
is waived or lost by any mistransmission. If you receive this message in error,
please immediately delete it and all copies of it from your system, destroy any
hard copies of it securely and notify the sender. You must not, directly or
indirectly, use, disclose, distribute, print, or copy any part of this message
if you are not the intended recipient. STADIUM GROUP PLC and any of its subsidiaries
each reserve the right to monitor all e-mail communications through its networks.
Any views expressed in this message are those of the individual sender, except where
the message states otherwise and the sender is authorised to state them to be the
views of Stadium Group Plc. or one of its subsidiaries.
Although this message has been scanned by MailMarshall for known viruses and
inappropriate content, we recommend that recipients employ appropriate measures on
their systems to intercept any such material.
Thank You - Stadium Group Plc., IT Department - Tel: +44 (0)1429 266544
#####################################################################################
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|