Can anyone supply typical values for the following thermal properties
of Biphenol Resins, as used for PED/PEM (particularly surface mount
package) moulding compounds?
I've searched all my usual sources, but only have figures for the
(more common?) Epoxy Cresol Novalac Resins:
Moulding Compound: TCE: Therm.Cond: Tg:
(ppm x 10^6/degC) (W/mdegC) (degC)
----------------------------------------------------------------------
Epoxy Cresol 16 0.67 155
Novalac Resin (some up to 20) (some up to 200)
Biphenol Resin ? ? ?
Thanks for any figures/information,
Regards all,
Clive ffitch
Matra BAe Dynamics (UK)
Stevenage, England
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|