TECHNET Archives

June 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 16 Jun 2004 11:33:48 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Rudy Sedlak <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
Most immersion Silver baths contain an anti-tarnish to prevent discoloration,
as you see, for instance on your silverware at home, if you have the
expensive stuff..

So, it could be a lack of, or lowered level, anti-tarnish in the plating
bath... most of the immersion silver baths use triazole as the anti-tarnish, and
there is a pretty easy test for triazoles from the Hach company, out of
Colorado.

If it is Copper showing through, as has been suggested, this could be because
the silver deposit is porous, which can come from plating on to a dirty
Copper surface...recall that the step before plating silver is to develop the
soldermask, which is an "iffy" process, and has been known to leave some material
behind.

If the surface is dirty, the silver will not adhere real well, and a tape
test would probably show that.

Regards,

Rudy Sedlak
RD Chemical Company

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2