TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 5 Jan 2006 12:57:44 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin Asbell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Franklin Asbell <[log in to unmask]>
Parts/Attachments:
text/plain (42 lines)
Received an unusual request for quote with a fab note callout for the
following.



1.      Plate 200/50 microinches SnAu (very hard)





Now I read that as 200 microinches of tin plating, followed by 50
microinches of Gold and thought to myself..huhhhh!!!



I contacted the buyer and he agreed it was quite unusual but they indeed
need gold over tin. The buyer could not explain why, so I thought I would
see if others have performed this process, and why such uncommonly mixed
coatings???



Franklin








---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2