Alan
But it's so obvious... but, then, so are many of the things we are
confronted with :-(
Brian
Alan Brewin wrote:
>
> Hallelujah!
>
> Nobody believes me when I tell them this Brian! We have seem this time and
> again with customers specifying a silicone because they want a 'more
> waterproof' coating. They always end up using so much more material to get
> the same performance.
>
> Alan Brewin.
> Concoat Ltd.
>
> -----Original Message-----
> From: Brian Ellis <[log in to unmask]>
> To: [log in to unmask] <[log in to unmask]>
> Date: 21 May 2000 10:26
> Subject: Re: [TN] Silicone Confromal Coating
>
> >Ken
> >
> >Just remember that silicone coatings are generally 2-10 times faster in
> >passing osmotic humidity for a given thickness than acrylic (best),
> >epoxy or polurethane, so the final protection against vesication is
> >considerably inferior, especially if it is a type that does not require
> >a special (aggressive) primer to ensure adhesion. Many think that,
> >because silicone coatings are water-repellent, they are also
> >moisture-repellent. Nothing is farther from the truth.
> >
> >Brian
> >
> >Ken Bloomquist wrote:
> >>
> >> Hi TechNet,
> >>
> >> We have a customer that wants us to spray Silicone confromal coating on
> >> their boards. We currently spray polyurethane and acrylic.
> >>
> >> My question is: Is there any problem adding Silicone to our process? What
> >> art the things we need to consider in adding this process?
> >>
> >> Thanks,
> >>
> >> Ken Bloomquist
> >>
> >> ##############################################################
> >> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> >> ##############################################################
> >> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> >> the body:
> >> To subscribe: SUBSCRIBE TECHNET <your full name>
> >> To unsubscribe: SIGNOFF TECHNET
> >> ##############################################################
> >> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> >> information.
> >> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> >> 847-509-9700 ext.5315
> >> ##############################################################
> >
> >--
> >Brian Ellis
> >Protonique SA
> >PO Box 78
> >CH-1032 Romanel-sur-Lausanne, Switzerland
> >Voice: +41 21-648 23 34 Fax: +41 21-648 24 11
> >E-mail: [log in to unmask]
> >URL: Technical and consultancy divisions:
> > http://www.protonique.com
> > Web services division:
> > http://www.protonique.com/webserv
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in
> >the body:
> >To subscribe: SUBSCRIBE TECHNET <your full name>
> >To unsubscribe: SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> >information.
> >If you need assistance - contact Keach Sasamori at [log in to unmask] or
> >847-509-9700 ext.5315
> >##############################################################
> >
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
--
Brian Ellis
Protonique SA
PO Box 78
CH-1032 Romanel-sur-Lausanne, Switzerland
Voice: +41 21-648 23 34 Fax: +41 21-648 24 11
E-mail: [log in to unmask]
URL: Technical and consultancy divisions:
http://www.protonique.com
Web services division:
http://www.protonique.com/webserv
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|