TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 19 May 2006 07:57:18 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Hi Suganthi,
Well, for some PCBs there is also a Ni overplate.
Basically, the processes after drilling the hole are:
1) desmear [either chemically or by plasma etching];
2) catalysation;
3) electroless Cu flash;
4) electrolytic Cu plate,
with rinse/wask steps in between.
The Cu flash is required for electrical continuity for the electrolytic
plating., which is carried out, very basically in an acid solution with the PCB as
cathode between Cu-anodes from which the plating process removes Cu in ion
form which move in the solution to the PCB and deposit as Cu-plating.
The plating current density determines the rate of plating, additives
determine how fast you can plate and still get Cu-plating with good physical
properties. This is it in an nutshell--in practice things get more complicated.



Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2