The primary function is to prevent solder deposition to preselected sites
during the machine(wave)soldering operation.
These areas can be discrete components that require post hand soldering,
dimensional tolerance locations that can not have solder build up, hardware
sites; selective plated areas like gold key pads, connectors, switches etc.
It can also be used for such things as component tack down and as a
containment barrier to prevent solder from running to adjacent areas.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-356-6076
-----Original Message-----
From: S. Miller [mailto:[log in to unmask]]
Sent: Thursday, August 24, 2000 9:39 PM
To: [log in to unmask]
Subject: [TN] Functional Intent of Peelable Soldermask
To All,
I have been introduced to several projects in Europe, all requiring the
application of peelable soldermask.
Given that this is a disposable process (peelable soldermask is removed
after
PCBA), why bother with it at all?
What function does it serve? Is really required?
Any and all feedback on this issue would be truly appreciated.
Regards,
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|