This is good advise for highly active [low pH] liquid fluxes, but Joel is
asking about lead free solder paste.
The activity level in WS solder pastes is much lower, closer to ordinary NC
types.
[If the flux in paste were active enough to attack solder it would chew up
the powder in the jar, making the paste useless].
Well formulated water wash pastes are able to take a delayed wash cycle
permitting cleaning to take place after a couple of reflows (one each side)
or post reflow component attach and repair, thus allowing a single wash
after all assembly.



Regards

Mike Fenner
Indium Corporation

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: 19 January 2006 08:50
To: [log in to unmask]
Subject: Re: [TN] Time before Cleaning WS Flux

As a general rule, water-soluble flux residues are very dangerous. They are
usually very acid and can attack metals on the assembly. At the best they
will make the solder joints matt. At the worst, increasing quantity of the
residues will form adsorption bonds with the substrate and components within
the residues may polymerise, making it quasi-impossible to clean the
residues after, say, an hour or so. It therefore is **very** necessary that
cleaning be started within minutes of soldering. However, there is an
excellent work-around that has been proven and that can extend the hold time
before cleaning to a few hours, the use of a chelating neutraliser. Many
flux manufacturers offer these under trade names such as Neutralizer 2051,
Rinse-Aid and so on. They are mildly alkaline, buffered, room-temperature,
dilute baths (pH typically 8.5 to 9), which must NOT be confused with
saponifiers, which are unsuitable for this job. They serve many functions,
but the assemblies can stay therein, immediately after soldering/reflow,
from 2 minutes up to, say, 4+ hours. They will actually improve the cleaning
quality at almost no cost. The assemblies should be cleaned within minutes
of their removal from the holding tank. The makers usually recommend a 5%
solution of the concentrate, but a 2% solution has been proved equally
effective.

You can see this technique being used on the old video at
http://www.protonique.com/video/ in the context of wave soldering.

Brian

Joel Mearig wrote:
> I am currently using a water-soluble, lead-free solder paste from
> Kester. I am trying to minimize the cleaning cycles so I leave flux on
> the product for an extended period of time. Do any of you have any
> recommendations on the amount of time flux can be left on the product
> without affecting the cleaning process? Thanks in advance for your input.
>
>
>
> Joel Mearig
>
> Delta Tau Data Systems, Inc.
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2