I'm not an ESD expert... so treat the following with caution, as it may not
be the same situation.
A similar concern was raised by a customer after I recommended forced air
cooling after reflow. "Floating body charging" or similar words.
Not being an expert and thinking this could be of more general concern, I
got a static expert and his gear and we spent an interesting few hours with
meters, ionizers, blowers, factory airlines and so on and found .....
nothing.
We rationalised that the stream carrying charges to the work, would
similarly allow a path from the work. That accidental gas ionizing was no
different (apart from the cash) to deliberate ionising.
Does this make sense?
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne - IIW
Sent: Tuesday, March 23, 2010 9:51 PM
To: [log in to unmask]
Subject: [TN] air or nitrogen for drying
We have a number of "airbrush" low pressure nozzles around here for spraying
solvents on reworked boards and for drying them off. I know that nozzles
can create static, but I have had no problems to date and have had no
problem with dust sticking to the boards when I dry them off this way.
I haven't been able to find anything on trying to quantify static from
nozzles used in this way. Does anyone have data? Moving to ionized
blow-off for drying the boards would be painful, as that means yet more
equipment in our small cleaning stations.
Wayne Thayer
________________________________
This e-mail and any files transmitted with it may be proprietary and are
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this e-mail in error please notify the
sender.
Please note that any views or opinions presented in this e-mail are solely
those of the author and do not necessarily represent those of ITT
Corporation. The recipient should check this e-mail and any attachments for
the presence of viruses. ITT accepts no liability for any damage caused by
any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|