Dear All,
For an 13.56 MHz antenna trace (25 mil wide & 400 mm long) running
between 2 pins of a differential transceiver (Tx1 & Tx2) we want to
maintain dimensional tolerance of + / - 10 % (trace width & trace thickness
including masking)? What has to be specified in the fabrication notes for
this?
There is no reference plane below this trace. How to ensure the
impedance tolerance is within 10 %? How should be the impedance coupon
designed for this purpose to do TDR measurements?
Sincerely
K.Balasubramanian
Project Leader - Hardware.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------