Dear Mr. Patel:
Could you provide additional detail regarding the nature of the problem?
Evaluating SEM/EDX data is tricky, but based upon the information you
provided, possible sources for the elements identified would be:
1) Si - residue from a pumice scrub or silicon based anti-foam;
2) S - potentially from a HAL flux or copper pre-clean product prior to
HAL;
3) O and C - these elements are present in LPI, in HAL fluids (both
in the polyol and organic acids), and in the epoxy laminate;
hence difficult without quantitative data to speculate on
a source;
4) Ca - most probably from city or "tap" water used for rinsing (hard
water scale is likely calcium carbonate (CaCO3), which
would also be a source for carbon and oxygen);
5) Cl - again would be present in city water, but could also be present
in hydrochloric acid activated HAL fluxs; and
6) Ba - ?????
Good luck!
Regards,
Ted Stern
Ken Patel wrote:
>
> Dear Technetters,
>
> I need all possible help to understand SEM analysis done on my board and to
> find out possible sources of basic elements.
>
> (1) On solder mask area, there was Silicon (Si), Sulfur (S) - is it due to
> LPI solder mask? Also found Oxygen (O) and Carbon (C)- meaning flux residue?
>
> (2) Found Silicon (Si), Chlorine (Cl), Calcium (Ca), Barium (Ba), Oxygen (O)
> and Carbon (C) on epoxy and in a kind of void area- is it from flux?
>
> Is there any book that help me solve above mystery?
>
> re,
> ken patel
>
> ______________________________________________________
> Ken Patel Phone: (408) 490-6804
> 1708 McCarthy Blvd. Fax: (408) 490-6859
> Milpitas, CA 95035 Beeper: (888) 769-1808
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|