Blair;
I have a white board in my office that has had notes on it for at least
the past 6 months. I just attempted to clean it after reading your post, and
I can see your frustration. I was able to clean off the old stuff with stamp
pad ink reactivator. It worked great compared to alcohol, or window cleaner.
It's nasty stuff though - Flammability = 3, Health = 1, Reactivity = 0,
Personal Protection = B. I'm not sure waxing would be a good idea, it may
prevent the dry erase markers from writing on it at all. Maybe a small test
spot in a corner with your favorite wax would be a good test. My favorite
window cleaner is Rain-X. It will provide a protective film that makes rain
bead up and run off. Maybe you can test it on a corner of one of your
boards. I've found it at most auto supply stores. I usually buy the
concentrate and mix a capful with a quart of water. Good luck!
Dave Simonik
Sanmina - SCI
Owego NY Division
-----Original Message-----
From: Blair K. Hogg [mailto:[log in to unmask]]
Sent: Friday, June 17, 2005 8:27 AM
To: [log in to unmask]
Subject: [NTC] - (Sort of) Need help from the chemical gurus out there
I thought this would be a good question for Friday, not related to lead in
solder or anything similar....
We have a training / breakout room with large white boards on the walls. The
standard cleaner works OK for removing the markings left on for days or
weeks, but some still remains. Is there a better cleaning solution (not
likely, you would think that the experts in white board markers would know
how to remove this stuff if it sits dried for a while) that will clean these
boards?
Second question - can the white boards be waxed periodically to improve
their cleaning performance? What type of wax would be best?
Happy Friday,
Blair
*******************************************************************
This email and any files transmitted with it are confidential and intended
solely for the use of the individual or entity to whom they are addressed.
If you have received this email in error please notify the system manager.
This footnote also confirms that this email message has been swept for the
presence of computer viruses.
www.hubbell.com - Hubbell Incorporated
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
____________________________________________________________________________
_
Scanned by Sanmina-SCI eShield
____________________________________________________________________________
_
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|