The aluminum ( aluminium ) does not touch the junction. The tape that I was
talking about has a paper backing and fairly thick adhesive.
-----Original Message-----
From: Dave Dixon [mailto:[log in to unmask]]
Sent: Friday, 12 August 2005 8:31 AM
To: [log in to unmask]
Subject: Re: [TN] Aluminum Tape for Profiling
Can you use a dissimilar metal alloy
at the thermocouple junction without
causing problems? That just doesn't
seem right to me.
Dave
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ofer Cohen
Sent: Friday, August 12, 2005 8:22 AM
To: [log in to unmask]
Subject: Re: Aluminum Tape for Profiling
... But, at the end of the day, the best bonding (from point of view of
thermal resistance and measurement accuracy) is to solder the thermo couple
to the measured pad using high temp solder. The tapes and adhesives shall be
used only as strain relievers.
Ofer Cohen
Quality and Technology manager
Seabridge - a Siemens company
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Charles Caswell
> Sent: Friday, August 12, 2005 14:23
> To: [log in to unmask]
> Subject: Re: [TN] Aluminum Tape for Profiling
>
> You can also try the local hardware store where they have duct tape.
> It does stick very well but after heating a little alcohol will remove
> the residue.
>
> -----Original Message-----
> From: Dave Dixon [mailto:[log in to unmask]]
> Sent: Thursday, 11 August 2005 10:31 AM
> To: [log in to unmask]
> Subject: Re: [TN] Aluminum Tape for Profiling
>
> Omega offers "Thermcoat" adhesive for this purpose. It may be too
> permanent for your needs though. Just my 2 ¢.
> Dave
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Barr, Bob
> Sent: Thursday, August 11, 2005 9:58 AM
> To: [log in to unmask]
> Subject: Aluminum Tape for Profiling
>
> Does anybody have a source for the aluminum tape recommended by KIC
> and others for attaching thermocouples? I know KIC sells it, but their
> price seems very high.
>
> Thanks.
>
> Bob
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of previous
> posts
> at: http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail
to [log in to unmask]: SET Technet Digest Search the archives of previous posts
at: http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|