Gerald,
I suspect ACI Technologies has some data on this, though I don't have it
at my fingertips. Try Fred Verdi: [log in to unmask]
Li, Poranki, Srihari et al at SUNY Binghamton coauthored a paper with a
couple of Sanmina-SCI folks at SMTAI in 2009: "Reliability Assessment of
Reballed BGAs." A quick Google search suggests lots of places have
decided to "borrow" it from SMTA ( :-) )
Here's one:
ftp://wilbur.eng.auburn.edu/pub/zhangj2/experiment%20paper/reliability%2
0assessment%20of%20reballed%20BGAs.pdf
There also are described methods that avoid some of the heat cycles
associated with desoldering and resoldering.
BEST has written about its manual wicking braid process, which
eliminates one of the thermal excursions:
http://circuitsassembly.com/cms/component/content/article/201/8397-bga-r
eballing-reliability
And our (TechNet, I mean) own Dean Stadem has written about a laser
method that avoids two thermal excursions:
http://circuitsassembly.com/cms/component/content/article/199/7193-solde
r-ball-attachment-using-laser-soldering
Best,
Mike
Mike Buetow
Circuits Assembly
w/m 617-327-4702
>>> The CIRCUITS ASSEMBLY EMS Directory -- over 2,100 listings, in Excel
www.circuitsassembly.com/dems <<<
Follow me on Twitter: twitter.com/mikebuetow
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerald Bogert
Sent: Wednesday, June 01, 2011 3:22 PM
To: [log in to unmask]
Subject: [TN] Re-balling BGAs
June 1, 2011
Anyone have technical data to support (or not support) re-balling of
BGAs to change from SAC balls to Pb balls???
My understanding is that because of the extra heat cycle involved, BGA
manufacturers may not stand behind their part warranty if re-balling is
done. I also seem to recall a technical poster or paper presented at
IPC several years ago which I believe indicated a reduction in
reliability of the part if it is re-balled.
Also seems to me that if one were to re-ball a BGA, this would be a
repair and not a reqork process and as such may require specific
customer approval.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|