TECHNET Archives

May 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Alan Brewin <[log in to unmask]>
Date:
Fri, 26 May 2000 18:28:08 +0100
Reply-To:
Mik Fenner <[log in to unmask]>
Subject:
From:
Mik Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
Organization:
BSAP
MIME-Version:
1.0
Parts/Attachments:
text/plain (57 lines)
Yep it does seem odd, but here's how I would rationalise it:

plasma etching could be doing two things:
1) activating surface to improve poor adhesion
2) reducing effects of moisture ingression when it does reach surface.

Course, if you had a better adhering  more protective product then maybe you could dispense with
the plasma......

Mike Fenner




----- Original Message -----
From: Alan Brewin <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, May 26, 2000 11:41 AM
Subject: Re: [TN] Solder Mask


> Jerry,
>
> It just doesn't make sense (to me anyway) to go to the effort of plasma
> etching to get adhesion, and they to use a silicone material. Silicones
> generally do not have good adhesion. I feel sure that if you use an acrylic
> or urethane material (providing your board is pretty clean) you won't have
> to plasma etch.
>
> Your comment about rework surprises me, I may be missing something? It has
> always been my experience that acrylics are a lot easier to re-work than
> silicones/RTV's. Do you want to chemically remove/rework or are you
> soldering straight through the product?
>
> I also agree with Brian about the danger of relying upon reported dielectric
> properties of a material measured at STP rather than at higher humidity if
> these
> conditions will exist in your end application.
>
> Alan Brewin
>
> Concoat Ltd

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2