Another solution to look at is an anti-tombstoning paaste produced by
Multicore. It is a blended powder of two alloys and sizes that seems to
really work.
>
>
> Hello to All,
>
> We have had tombstoning in a Film Chip Capacitor (Size 1206).
> It is being soldered in a normal reflow process, and this is the only
> component that it is showing tombstoning.
> Reviewing the specs. of the component in the web I found that this
> capacitor is recommended for Wave Soldering.
> Does anyone know the difference in construction between the Capacitors for
> Reflow and Wave Soldering?
> Is it possible that this be cause for the tombstoning?
> I am also sending pictures for cross section for the capacitors that we are
> using (Recommended for Wave Soldering).
> They could be seen at Steve's site.
>
> Regards
>
> Alejandro Becerra
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------