TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 27 Jul 2011 14:01:31 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Victor Hernandez <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (109 lines)
Chris,

   Can this spec apply to gold finger plating on Printed Circuit Boards?

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Wednesday, July 27, 2011 11:23 AM
To: [log in to unmask]
Subject: Re: [TN] hard gold verification

Thank you very much Anil.
You confirm my suspicion and give me confidence to recommend to my customer to dig deeper (as the others have suggested, on and off-line).
I will also recommend MIL-DTL-45204 type qualification and periodic conformance.
Chris

-----Original Message-----
From: Anil kher [mailto:[log in to unmask]] 
Sent: Saturday, July 23, 2011 5:26 AM
To: Chris Mahanna; [log in to unmask]
Subject: RE: hard gold verification

To test hard gold on plating of 1 to 4  micron is not easy. Procedure is - a supplier with very reliable process control and proper documentation of bath maintenance.
Then every 6 months you get a 40 micron gold plated sample and do a test on micro hardness. Then if the bath is maintained at same levels you get reliability. The tracking of Co content is ok to maintain control. Nickel in plating is poor bath working - may be new supplier - whose nickel plating bath is getting dragged into the gold.

Yr customer shd be worried abt wear resistance than pure hardness. If its serious business get in touch offline Anil Kher

Managing Director
Micro Interconnexion Pvt. Ltd.
D3-12A Corlim Ind. Estate, Corlim, ILHAS Goa, India, 403110
+91-832-2284209/ 337
alt email : [log in to unmask]

LEADERS IN GOLD PLATED PCBs




-----Original Message-----
From: Chris Mahanna [mailto:[log in to unmask]]
Sent: Thursday, July 21, 2011 9:51 PM
Subject: hard gold verification

Hello netters

We are an independent test facility.  Occasionally we are asked to verify hard gold as part of bare board qualifications.
Our customers in these cases are usually the OEM supply chain QA.  The buyer controls the source and Quality's only prayer is to run some first articles through a 3rd party.
Our customer's chance of determining the hard gold formula used on his boards is slim to none.  If it weren't for UL, they probably wouldn't even know who supposedly built them.

Some time ago, we tried Nano-indentation and there is a related TechNet thread.  It didn't work for us.
I assumed wear studies might be cost prohibitive, so we went to looking for 0.2% cobalt by SEM-EDS.  This has worked nicely, until today.

Today we have 0.09% Co and 0.07% Ni.  From what I read, 0.1 Co is easily explained by too rapid deposition, and hardness suffers greatly.  The question is whether the Ni is supposed to be there as a hardener or not?  If yes, then 0.16% total is probably in the ballpark.  But what are the chances it just got dragged there?  Does it matter?

Thanks in advance

Chris


Chris Mahanna
Robisan Laboratory Inc.




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2